PENGARUH PENAMBAHANAN METAKAOLIN DAN SUPERPLASTICIZER TERHADAP KUAT TEKAN BETON PADA MUTU K-400

Masri A Rivai, RA Sri Martini, Erdin Dimas

Abstract


High-quality concrete usually uses an addition to workaholic, high-pressure, and concrete durability such as metacaolin and superplasticizer.
The Study was conducted to find out how the metacaolin + superplasticizer addition to the strong K-400 press of concrete. The test object used was a cube 15 x 15 x 15 cm. Strong tests of concrete were made at the age of 3 days, 14 days, and 28 days. The research is done on normal concrete, and metacaolin 10% + superplasticizer 0,5%, 1%, 1,5%, 2%, 2,5%, 3%, and 3,5% with separate parts.
Research shows the strong value of normal concrete pressure at 28 days on 403,66 Kg/cm² while strong value of optimum concrete at 28 days occurs in a variety of Metacaolin 10% + Superplastizer 3% on 460,58 Kg/cm². It is known that adding metacaolin + superplasticizer add to strong concrete pressure.

Key Words : concrete, metacaolin, superplasticizer, and strong press.


Full Text:

PDF


DOI: https://doi.org/10.32502/jbearing.3656202171

Refbacks

  • There are currently no refbacks.


Creative Commons License
This work is licensed under a Creative Commons Attribution-ShareAlike 4.0 International License.

Published by :

Program Studi Teknik Sipil, Universitas Muhammadiyah Palembang

P-ISSN : 2085-6261

E-ISSN : 2623-1409

Email : bearing@um-palembang.ac.id 

 Creative Commons Licence

Bearing : Jurnal Penelitian dan Kajian Teknik Sipil is licensed under a Creative Commons Attribution-ShareAlike 4.0 International License.